Nickel Alloy C263 Round Bar, Nickel Alloy C263 Round Bar Importers, Nickel Alloy C263 Round Bar Suppliers, Nickel Alloy C263 Round Bar Exporter, Nickel Alloy C263 Round Bar Stockists.
Nickel Alloy C263 Round Bar in India, Nickel Alloy C263 Round Bar Importers in India, Nickel Alloy C263 Round Bar Suppliers in India, Nickel Alloy C263 Round Bar Exporter in India, Nickel Alloy C263 Round Bar Stockists in India.
Nickel Alloy C263 Round Bar in Mumbai, Nickel Alloy C263 Round Bar Importers in Mumbai, Nickel Alloy C263 Round Bar Suppliers in Mumbai, Nickel Alloy C263 Round Bar Exporters in Mumbai, Nickel Alloy C263 Round Bar Stockists in Mumbai.
Hastelloy C-263, is an age hardenable nickel-cobalt-chromium-molybdenum alloy. Also known as Nickel Alloy C-263 and Haynes® 263, Hastelloy® 2 C-263 has some very positive attributes that make it ideal for a wide range of applications. These attributes include:
- Very good aged strength properties
- Excellent fabrication characteristics in the annealed condition
- Good ductility, formability, and weldability
- Intermediate temperature tensile ductility
- Hot working temp range from 1750° to 2100° F (955°-1150° C)
- Can easily be welding using methods including TIG, MIG, electron beam and resistance welding
In order to be considered Hastelloy C-263, an alloy must have a chemical composition of:
- Ni 51%
- Cr 20%
- Co 20%
- Ti 2.15%
- Al .45%
- C .060%
A number of different critical industries rely on Hastelloy C-263 and Nickel Alloy C-263 for their applications including:
- Aircraft and Land-based turbine applications
- Low-temperature combustors
- Transition liners
- Ring components
- Welding of GTD222 investment castings
Continental Steel has been a distributor of Hastelloy C-263 and Nickel Alloy C-263 for many years, especially in wire form. It is also important to note that Hastelloy C-263 meets or exceeds various specifications including:
- UNS: N07263
- W. Nr./EN: 2.4650
- AMS: 5966(weld wire)
- GE: B50A771, B50A783
- RR: 9500/16
Chemical Composition (Weight %) | |||||||||||||||||
C | Mn | Si | P | S | Cr | Co | Mo | Ti | Al | Ti + Al | B | Fe | Cu | Ni | |||
Min | 0.04 | 19.00 | 19.00 | 5.60 | 1.90 | 0.30 | 2.40 | ||||||||||
Max | 0.08 | 0.60 | 0.40 | 0.015 | 0.007 | 21.00 | 21.00 | 6.10 | 2.40 | 0.60 | 2.80 | 0.005 | 0.70 | 0.20 | Bal |
Typical Mechanical Properties for bar (Min) | ||||||||||
Condition | Tensile Strength, KSI | Yield Strength 0.2%, KSI | Elongation % | Reduction of Area % | Hardness HB | |||||
Bar | 78.50 | 58.50 | 12 |