AMS 5537 Sheet, AMS 5537 Sheet Importers, AMS 5537 Sheet Suppliers, AMS 5537 Sheet Exporter, 718 Inconel Alloy Stockists.
AMS 5537 Sheet in India, AMS 5537 Sheet Importers in India, AMS 5537 Sheet Suppliers in India, AMS 5537 Sheet Exporter in India, 718 Inconel Alloy Stockists in India.
AMS 5537 Sheet in Mumbai, AMS 5537 Sheet Importers in Mumbai, AMS 5537 Sheet Suppliers in Mumbai, AMS 5537 Sheet Exporters in Mumbai, 7075 T6 Aluminium Alloy Stockists in Mumbai.
Cobalt L-605 (also known as alloy 25) is a cobalt-based superalloy with high levels of chromium and tungsten. It is characterized by outstanding high-temperature strength up to 1500 °F (1093 °C), excellent oxidation resistance at high temperatures up to 2000 °F (1093 °C) in corrosive environments, and superior resistance to sulfidation wear and galling. Cobalt L-605 has other less-known qualities like high ductility and biocompatibility. Cobalt L-605 is non-magnetic.
Chemical Composition of Cobalt L-605
Element | Min (%) | Max (%) |
Carbon, C | 0.05 | 0.15 |
Manganese, Mn | — | ≤ 2.00 |
Silicon, Si | — | ≤ 0.40 |
Sulfur, S | — | ≤ 0.015 |
Phosphorus, P | — | ≤ 0.02 |
Chromium, Cr | 19.0 | 21.0 |
Molybdenum, Mo | 1.20 | 1.40 |
Iron, Fe | — | ≤ 3.00 |
Tungsten, W | 14.0 | 16.0 |
Nickel, Ni | 9.0 | 11.0 |
Cobalt, Co | — | *Balance |
Mechanical and Physical Properties
Property | Imperial | Metric |
Density | 0.335 lb/in3 | 9.27 g/cm3 |
Melting Range | 2425 – 2570 °F | 1330 – 1410 °C |
Tensile Strength | 154 ksi | 1061 MPa |
Tensile Strength, Yield 0.2% | 75 ksi | 517 MPa |
Elongation in 2 inches (50 mm) | 55 % | 55 % |
Elongation A5 | 25 % | 25 % |
Electrical Resistivity | 34.9 µΩ in | 88.6 µΩ cm |
Magnetic Permeability at 200 oersteds | 1.002 | 1.002 |
Thermal Conductivity | 65 Btu⋅in/ft2 h °F | 9.4 W/m K |
Specific Heat | 0.092 Btu/lb °F | 385 J/kg °C |
Coefficient of Thermal Expansion, RT – 200°F | 6.8 × 10-6 in/in °F | 12.3 µm/m °C |
Resistance on air (up to the temperature listed) | 1994 °F | 1090 °C |