L605 Round Bar, L605 Round Bar Importers, L605 Round Bar Suppliers, L605 Round Bar Exporter, L605 Round Bar Stockists.
L605 Round Bar in India, L605 Round Bar Importers in India, L605 Round Bar Suppliers in India, L605 Round Bar Exporter in India, L605 Round Bar Stockists in India.
L605 Round Bar in Mumbai, L605 Round Bar Importers in Mumbai, L605 Round Bar Suppliers in Mumbai, L605 Round Bar Exporters in Mumbai, L605 Round Bar Stockists in Mumbai.
Haynes 25 is a Cobalt-Nickel-Chromium-Tungsten alloy that combines features like strength, high-temperature tolerance, excellent resistance to sulfidation, and galling. Haynes alloy 25 is heavily used in industrial applications and gas turbine parts.
Hastelloy 25 is fabricated and formed by usual conventional techniques, which also helps in the casting of the alloy. The excellent resistance to metal galling makes the alloy more useful. The high strength properties of this L605 alloy can be obtained through cold work. It is generally melted by vacuum induction or electro-slag remelting techniques. Haynes 25 remain nonmagnetic in various applications.
Common Names:
- Haynes 25
- Alloy L605
- UNS R30605
Executive Standards:
Rod, Bar, Wire, and Forging Stocks
- AMS 5759
- ASTM F90 GE
- B50T26A
Plate, Sheet, and Strip
- AMS 5537
Welding Wire and Coated Electrodes
- AMS 5759
- AMS 5796
- AMS 5797
Chemical Properties:
Chromium (%) | 19-21 |
Nickel (%) | 9-11 |
Tungsten (%) | 14-16 |
Iron (%) | Max 3 |
Manganese (%) | Max 2 |
Others (%) | Remainder |
Mechanical Properties:
Yield Strength (MPa) | Min 310 |
Yield Strength (ksi) | Min 45 |
Tensile Strength (MPa) | Min 862 |
Tensile strength (ksi) | Min 125 |
Break Elongation | Min 30% |
Elasticity Modulus (GPa) | 225 |
Elasticity Modulus (psi) | 32.6 x 106 |
Hardness
(BHN) |
250-275 |
Physical Properties:
Density | Lb/in3 | 0.327 |
g/cm3 | 9.07 | |
Melting Point | oF | 2425-2570 |
oC | 1330-1410 | |
Specific Heat | Btu/lb-oF | 0.096 |
J/kg-oC | 403 | |
Expansion Coefficient | 25-100oC | 12.8 |
70-200oF | 7.1 | |
Thermal Conductivity | W/m-oC | 10.5 |
BTU-in/hr-ft2–oF | 72 | |
Electrical Resistivity | µohm-cm | 88.6 |
µohm-in | 34.9 |